Hits: 686 img
Switching Waterborne Silicone Release Coatings for PET Film
Solids content helps estimate how much liquid you will handle and how much dry matter might remain. It does not show whether an emulsion will coat your PET evenly, cure in the existing oven or transfer to the back of the film after winding. When requesting a quote, start with the film, the coating line and the adhesive used in lamination.
Line conditions to share with suppliers
If line speed and oven length are fixed, tell the supplier how long the film actually spends in the oven. The oven setpoint alone does not tell you the temperature the film surface reaches. Even when two emulsions have the same nominal solids, check each supplier's application conditions.
|
What to share when requesting a quote |
What to check in the coating trial |
|
PET grade, thickness, coating side and surface treatment |
Check uniformity, dewetting, bare spots and whether the cured coating rubs off. |
|
Coater, line speed, oven and any measured film surface temperatures |
Check whether the existing line can produce a stable coating and log any adjustments. |
|
Actual adhesive, peel speed and acceptance limits |
Compare release force under the same conditions and check how well the adhesive bonds after peeling. |
|
Winding conditions, storage time and delivery format |
Look for blocking or possible transfer on unwinding and recheck the agreed limits after storage. |
IOTA 2121E silicone release emulsion for PET coating
The product page lists IOTA 2121E as a release emulsion for substrates including PET film and gives a solids content of 40%. That figure helps identify the grade as supplied. Verify the film surface, coating equipment and cure conditions on your line before setting a mix ratio or line speed.
Cost per usable square metre after a successful trial
Use PET from the same batch and the same adhesive, with the current coating as a control. If the new coating requires a lower line speed or a higher dry coat weight, or results in more rejected rolls, the price per kilogram can understate the cost of switching. Record actual consumption, usable area and line speed. The solids in the product as supplied are not necessarily the amount of effective silicone deposited on the film.
Keep sample evaluation and purchasing separate. Trial records show how the material runs on the line; purchase documents specify product identity, supply specifications, batch documentation and change notification. IOTA Silicone Oil (Anhui) Co., Ltd. provides solutions across the silicone value chain. We can help check candidate materials and product data against your substrate and line conditions. We do not provide complete formulations or formulation development services.
Frequently asked questions
Q1 Can I switch directly if both emulsions are 40% solids?
Check how solids content is defined and the form in which each product is supplied. Then verify wetting, cure, coating adhesion and performance with the actual adhesive.
Q2 Is meeting the release force spec enough for approval?
Also check the adhesive's bond after peeling and the roll's performance after winding and storage, against project requirements.
Q3 Can a small coupon replace a full roll trial?
A coupon can screen candidates. For roll production, verify continuous coating, oven conditions and winding.
Q4 Is the oven setpoint enough?
Also send the line speed, effective oven length and any available film surface temperature data to establish the actual heat exposure.
Q5 Does a product listed for PET automatically suit my project?
It is a candidate. Confirm the combination of film surface, equipment and adhesive in a line trial.